Comparison of shear bond strength of composite, compomer and resin modified glass ionomer in primary and permanent teeth: an in vitro study.

dc.contributor.authorPrabhakar, A Ren_US
dc.contributor.authorRaj, Sen_US
dc.contributor.authorRaju, O Sen_US
dc.date.accessioned2003-09-02en_US
dc.date.accessioned2009-06-02T09:34:59Z
dc.date.available2003-09-02en_US
dc.date.available2009-06-02T09:34:59Z
dc.date.issued2003-09-02en_US
dc.description.abstractThe aim of this study was to determine the difference in shear bond strength between Composite, Compomer and Resin modified glass ionomer cement in primary and permanent teeth. Thirty extracted primary molars and thirty premolars were selected and buccal surfaces of all the teeth were made smooth with the help of 300 grit silicon carbide paper. These specimens were then divided into 6 groups. Restorative materials were placed on the buccal surfaces of respective specimens with the help of acrylic template. All the specimens were subjected to thermocycling and shear bond strength was tested under the Honsfield testing machine and results were recorded in megapascals (MPa). The resultant scores were tabulated and statistically analysed. It was observed that in case of primary teeth resin modified glass ionomer exhibited significantly higher shear bond strength as compared to composite and compomer, where as on permanent teeth composite demonstrated a significantly higher shear bond strength than that of the resin modified glass ionomer and compomer, where as compomer gave poor shear bond strength in both primary and permanent teeth.en_US
dc.description.affiliationDepartment of Pedodontics and Preventive Dentistry, Bapuji Dental College and Hospital, Davangere, Kamataka, India.en_US
dc.identifier.citationPrabhakar AR, Raj S, Raju OS. Comparison of shear bond strength of composite, compomer and resin modified glass ionomer in primary and permanent teeth: an in vitro study. Journal of the Indian Society of Pedodontics and Preventive Dentistry. 2003 Sep; 21(3): 86-94en_US
dc.identifier.urihttps://imsear.searo.who.int/handle/123456789/114996
dc.language.isoengen_US
dc.source.urihttps://medind.nic.in/jao/jaoaj.shtmlen_US
dc.subject.meshBicuspiden_US
dc.subject.meshCompomers --chemistryen_US
dc.subject.meshComposite Resins --chemistryen_US
dc.subject.meshDental Bonding --methodsen_US
dc.subject.meshDental Stress Analysisen_US
dc.subject.meshDentition, Permanenten_US
dc.subject.meshGlass Ionomer Cements --chemistryen_US
dc.subject.meshHumansen_US
dc.subject.meshMaterials Testingen_US
dc.subject.meshMolaren_US
dc.subject.meshResin Cementsen_US
dc.subject.meshShear Strengthen_US
dc.subject.meshTooth, Deciduousen_US
dc.titleComparison of shear bond strength of composite, compomer and resin modified glass ionomer in primary and permanent teeth: an in vitro study.en_US
dc.typeComparative Studyen_US
dc.typeIn Vitroen_US
dc.typeJournal Articleen_US
Files
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
1.79 KB
Format:
Plain Text
Description: